Remove carbon deposits and other impurities from glass making and rubber tire molds without damaging the surface or critical edges. Remove burrs from the thin seal.
Ball jet treatment is applied to black and non-black objects, including aircraft engine blades, integral blades, turbines, etc. Shot Peening treatment for internal and external threads. Compress plasma coating.Main technical indicators
Manufacturing Process |
ZrO2 |
SiO2 |
AI2O3 |
59%-62% |
26%-29% |
9%-12% |
Main components:
Level |
Main Chemical Index % |
||
ZrO2 |
SiO2 |
Al2O3 |
|
P-B Series(for Sandblasting) |
60-62 |
24-30 |
6-12 |
J-B Series(for Sandblasting) |
62-65 |
24-30 |
4-10 |
Z Series (for shot peening) |
62-65 |
24-30 |
4-10 |
Physical Index |
|
True density |
3.85 g/cm3 |
Bulk density |
2.3g/cm3 |
Vicker hardness |
700 HV |
B/Z20:0.600-0.850mm B/Z 40:0.250-0.425mm B/Z 80:0.125-0.212mm B/Z 120:0.063-0.125mm B/Z 170:0.045-0.090mm |
B/Z30:0.425-0.600mm B/Z 60:0.150-0.300mm B/Z 100: 0.106-0.180mm B/Z 150: 0.053-0.106mm B/Z 205:0.000-0.063mm |